    1, Possible reasons for thin phosphorizing film.
    The temperature is too low.
    Total acid value is too low.
    Free acid value is too high.

    2, Workpieces should be removed from the production line before the manufacturing is stoped.

    3, If mottling phenomenon happens on the surface.
   Keep the workpieces moist in transition of different working procedures.
   Check whether PH value is in normal range before phosphorizing.

    4,Tank liquor is reduced by deslagging.

    5, Wash at least twice after phosphorizing.